The aim of the present study was to examine the marginal adaptation of a new low-shrinkage siloranebased composite material (Filtek™ Silorane, 3M-Espe) by comparing it with a methacrylate-based composite material (CeramX™, Dentsply DeTrey). In particular, we wanted to test the hypothesis that reduced polymerization shrinkage would improve the marginal adaptation. Seventy-two patients participated in the study. A total of 158 restorations were placed in 80 premolars and 78 molars. Only Class II restorations were included, and each patient could contribute with more than one tooth. The restorations were scored at baseline and after one year. While statistical comparison of marginal adaptation at follow-up indicated better performance of CeramX™ both occlusally and approximally (p=0.01 and p<0.01), the low kappa value (32%) reflects the difficulty to assess marginal adaptation clinically. The reduction in polymerization shrinkage demonstrated in the laboratory was not clinically significant in the present study.
Clin Oral Invest (2011) 15:291–295 DOI 10.1007/s00784-010-0446-2 Received: 26 January 2010 / Accepted: 1 July 2010 / Published online: 20 July 2010
اگر شما نسبت به این اثر یا عنوان محق هستید، لطفا از طریق "بخش تماس با ما" با ما تماس بگیرید و برای اطلاعات بیشتر، صفحه قوانین و مقررات را مطالعه نمایید.

دیدگاه کاربران


لطفا در این قسمت فقط نظر شخصی در مورد این عنوان را وارد نمایید و در صورتیکه مشکلی با دانلود یا استفاده از این فایل دارید در صفحه کاربری تیکت ثبت کنید.

بارگزاری