The characterization of dentin defects produced by air polishing

The characterization of dentin defects produced by air polishing

  • نوع فایل : کتاب
  • زبان : انگلیسی
  • مؤلف : Kazuhiro Tada • Suphasiriroj Wiroj • Michitomo Inatomi • Soh Sato
  • چاپ و سال / کشور: 2011

Description

The objective of this study is to characterize the defects in the dentin surface after air polishing for three types of polishing powders and five different nozzle distances. Human teeth were embedded in acrylic resin and then polished until the dentin surface became exposed. The nozzle of the polisher was fixed at a specified distance (2, 3, 4, 5, or 6 mm) and orientation (45) with respect to the dentin surface. The three powders were CLASSIC (NaHCO3, 65 lm diameter), PERIO (glycine, 25 lm diameter), and SOFT (glycine, 65 lm diameter). With respect to nozzle distance, we find a significant difference in the mean defect depth only at 6 mm. The spray distance of 6 mm produced the shallowest defect depths. This variable had no effect on the defect volume. SOFT powder had significantly less depths and volumes of defects than the other two powders. The contact angle of the dentin increased significantly in all polishing tests, compared to an unpolished dentin surface (control). We find that spray distance of 6 mm from the nozzle of the polisher and orienting on 45 angle produced less dentin surface defects than any other distance in all powder systems used. At this distance, SOFT powder produced statistically significant smaller depth and volume defects than the other two powder groups.
Odontology DOI 10.1007/s10266-011-0019-0 Received: 26 October 2010 / Accepted: 24 December 2010
اگر شما نسبت به این اثر یا عنوان محق هستید، لطفا از طریق "بخش تماس با ما" با ما تماس بگیرید و برای اطلاعات بیشتر، صفحه قوانین و مقررات را مطالعه نمایید.

دیدگاه کاربران


لطفا در این قسمت فقط نظر شخصی در مورد این عنوان را وارد نمایید و در صورتیکه مشکلی با دانلود یا استفاده از این فایل دارید در صفحه کاربری تیکت ثبت کنید.

بارگزاری